Related Posts
How Much Air Do You Need For Your Abrasive Blast Process?
Return How Much Air Do You Need For Your Abrasive Blast Process? Abrasive Blast Process Air Consumption FAQs When it comes to air consumption for your abrasive blast process, how
Abrasive Blast System Sizing Guide
Abrasive Blast System Sizing Guide With Blue Dog Blasting on your team, you have access to the sandblasting expertise that only comes with decades of sandblasting experience. The table below
Iron Grit Abrasive
Mohs Hardness: 7 Bulk Density: 160 lbs cuft Hard, Heavy good etching abrasive Breaks down in small angular pieces Wear on nozzles and hoses Angular Shaped / Dark Grey or…
Contractor Thread vs. Standard Thread
Return Contractor Thread vs. Standard Thread We carry several different nozzle couplings on our site. From aluminum to nylon; standard coupling to threaded quick coupling; contractor to standard thread, we
Nozzle Comparison with Rust Removal
This test features the XL Performance Nozzle, Double Venturi Nozzle and the Long Venturi Nozzle. Each is being fed 90 PSI with an Empire 650 XL Sandblast Pot.
Crushed Glass
Mohs Hardness: 5.5-6.6 Bulk Density: 100 lbs cuft Made of 100% Recycled Glass Safe For Use Around Water American Made Contains less than 1% free silica Non-reactive & inert Beryllium…