Related Posts
Brown Aluminum Oxide
Mohs Hardness: 8-9 Bulk Density: 110 lbs cuft Hard and long lasting abrasives Typically used in blast cabinet and rooms because of recyclability Used in Vibratory Media as a cutting…
How Much Air Do You Need For Your Abrasive Blast Process?
Abrasive Blast Process Air Consumption FAQs? When it comes to air consumption for your abrasive blast process, how much is enough? How much compressed air do you really need for
Operator Review of Farrow Flow® Insert for Abrasive Blasting
Return Operator Review of Farrow Flow® Insert for Abrasive Blasting If someone told you they could install a product on my sandblast equipment in minutes, and it would both improve
Nozzle Comparison with Rust Removal
This test features the XL Performance Nozzle, Double Venturi Nozzle and the Long Venturi Nozzle. Each is being fed 90 PSI with an Empire 650 XL Sandblast Pot.
Silcion Carbide
Mohs Hardness: 9 Bulk Density: 95 lbs cuft Hardest of Non-Metallic Abrasives Fast Cutting of Coatings Silicon carbide is a ceramic material with an excellent hardness Hard brittle grains shatter…
Ceramic Bead
Mohs Hardness: 8 Bulk Density: 150 lbs cuft Heavy/Dense spherical media Blast Cleaning, Shot Peening & Microblast Long lasting media that outlasts most abrasives 10-15X Cost effective - reduced consumption,…