Related Posts
Crushed Glass
Mohs Hardness: 5.5-6.6 Bulk Density: 100 lbs cuft Made of 100% Recycled Glass Safe For Use Around Water American Made Contains less than 1% free silica Non-reactive & inert Beryllium…
Spartan Sandblast Abrasive
Mohs Hardness: 7 Bulk Density: 95-100 lbs cuft Stronger and More Angular Narrow distribution 3-5X Less Breakdown to Garnet Decreased disposal / High recyclability 0% Free Silica Made in the…
Coal Slag Abrasive
Mohs Hardness: 7 Bulk Density: 110 lbs cuft Low Cost Abrasive 100% Recycled Byproduct Tests show to breakdown slowe/create less dust than Garnet Fast Cutting of Coatings and Rust
How Much Air Do You Need For Your Abrasive Blast Process?
Abrasive Blast Process Air Consumption FAQs? When it comes to air consumption for your abrasive blast process, how much is enough? How much compressed air do you really need for
Garnet Abrasive
Mohs Hardness: 6.5-7 Bulk Density: 140 lbs cuft Used in Sandblast and Waterjet Relatively Hard Mined Mineral Heavy Abrasive Requires Higher Pressures to be effective Less than 10% Mined in…
Abrasive Blast System Sizing Guide
Abrasive Blast System Sizing Guide With Blue Dog Blasting on your team, you have access to the sandblasting expertise that only comes with decades of sandblasting experience. The table below